Preliminary Investigation of Allowable Weld Defect Size and Orientation for DEMO Cooling Pipes

Azman Azka,Martin Mittwollen

IEEE Transactions on Plasma Science(2024)

Cited 0|Views0
No score
Key words
Codes,Finite element analysis,Welding,Stress,Standards,Cooling,Maintenance,DEMO,maintenance,nondestructive examination,numerical analysis,pipe defect