谷歌浏览器插件
订阅小程序
在清言上使用

Plasma enhanced atomic layer deposition of crystallized gallium phosphide on Si with tri-Ethylgallium and tri-tert-Butylphosphine

APPLIED SURFACE SCIENCE(2023)

引用 1|浏览40
暂无评分
摘要
25 similar to 30 nm thick polycrystalline gallium phosphide (GaP) films with high P / Ga atomic ratios were deposited on Si (10 0) using a plasma enhanced atomic layer deposition (PE-ALD) process with triethyl gallium (TEG), tritertiary butyl phosphide (tri-TBP), and atomic hydrogen. The key is chemical functionalization of the Si (10 0) surface since the wet-cleaned Si surface is nearly inert to TEG and tri-TBP. In-situ Auger spectroscopy was employed to identify the most successful functionalization which employed a gas phase mixture of atomic hydrogen and tri-TBP consistent with formation of a surface phosphide layer on Si(1 00); this layer efficiently nucleated the PE-ALD of GaP. The crystallinity and surface roughness of GaP films were tuned by controlling the pulse length of atomic H plasma, showing the self-limiting ALD film growth with 2.7 angstrom/cycle. The optimal crystallized GaP thin film on 6 degrees-miscut Si showed local epitaxy growth of homogeneous GaP epi-layers in transmission electron microscopy (TEM).
更多
查看译文
关键词
Gallium phosphide,Nucleation,Local epitaxy growth,Plasma enhanced atomic layer deposition,tri-TBP,TEGa
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要