谷歌浏览器插件
订阅小程序
在清言上使用

Metastable pitting corrosion behavior and characteristics of passive film of laser powder bed fusion produced Ti-6Al-4V in NaCl solutions with different concentrations

CORROSION SCIENCE(2023)

引用 36|浏览17
暂无评分
关键词
Laser powder bed fusion,Ti-6Al-4V,Pitting corrosion,Passive film,Vacancies