Raman Scattering Measurement of Suspended Graphene under Extreme Strain Induced by Nanoindentation.
Advanced materials(2022)
摘要
Graphene is known as a superstiff and extremely strong material. Hence, applying strains greater than 1% to graphene and simultaneously measuring changes in its physical properties has been challenging because of the limited methodologies for measuring both high strain and other physical properties. Here, Raman scattering measurement of suspended graphene under extremely high biaxial strain as large as 6.1% using an atomic force microscopy (AFM)-Raman spectroscopy measurement tool is reported. Nanoindentation is performed using AFM tips machined to have a flat top and a hole shape, resulting in a strained graphene area sufficiently large to enable the acquisition of a Raman signal. At the same time, the laser light is focused on the strained flat area of the graphene membrane. The Raman signals of the G and 2D bands of graphene are redshifted by 282 and 684 cm-1 , respectively, which is unprecedented for graphene. This measurement technique provides an effective methodology to measure variations in the physical properties of atomically thin materials under superhigh strain.
更多查看译文
关键词
graphene,nanoindentation,Raman scattering,superhigh strain
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要