Comparison of wire-arc and powder-laser additive manufacturing for IN718 superalloy: unified consideration for selecting process parameters based on volumetric energy density
The International Journal of Advanced Manufacturing Technology(2021)
关键词
Cladding,Additive manufacturing,Process parameters,Energy density,IN718 superalloy
AI 理解论文