A Novel Activation Method for Regulating Surface Characteristics and Flotation Performance of Smithsonite: XPS, SEM-EDS, AFM, ToF-SIMS and FT-IR Studies

Separation and Purification Technology(2025)

引用 0|浏览6
暂无评分
摘要
Smithsonite is a typical zinc oxide mineral, and the flotation index is not ideal for the recovery of smithsonite via sulfidization -xanthate flotation. In this study, Pb 2 + was used as an activator for the stepwise activation of smithsonite in a sulfidization -xanthate flotation system. Micro-flotation tests and various surface analytical assays were employed to investigate the effects of Pb 2 + stepwise activation on the flotation behavior and surface properties of smithsonite. The micro-flotation tests revealed that the flotation recovery of smithsonite reached 90.26 % after the stepwise activation of Pb 2 + at an appropriate concentration. X-ray photoelectron spectroscopy, scanning electron microscopy-energy-dispersive X-ray spectroscopy, atomic force microscopy, and time -of -flight secondary ion mass spectrometry indicated that abundant active sites of Pb components appeared on the smithsonite surface after Pb 2 + stepwise activation, which promoted the adsorption of S ions on the smithsonite surface. The increase in the proportion of the PbS component after sulfidization effectively enhanced the reaction activity of the mineral surface. Fourier-transform infrared spectroscopy and contact angle measurements showed that xanthate could be stably adsorbed on the smithsonite surface after Pb 2 + stepwise activation, thereby enhancing the surface hydrophobicity and flotation behavior of smithsonite. Therefore, Pb 2 + stepwise activation can promote sulfidization on the smithsonite surface, improve the reactivity and hydrophobicity of the mineral surface, and substantially increase the flotation index of smithsonite.
更多
查看译文
关键词
Zinc oxide mineral,Activation method,Surface characteristics,Flotation separation
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要