Atomic Layer Deposition For Gradient Surface Modification And Controlled Hydrophilization Of Ultrafiltration Polymer Membranes
ACS APPLIED MATERIALS & INTERFACES(2021)
摘要
In recent years, atomic layer deposition (ALD) has emerged as a powerful technique for polymeric membrane surface modification. In this research, we study Al2O3 growth via ALD on two polymeric phase-inverted membranes: polyacrylonitrile (PAN) and polyetherimide (PEI). We demonstrate that Al2O3 can easily be grown on both membranes with as little as 10 ALD cycles. We investigate the formation of Al2O3 layer gradient through the depth of the membranes using high-resolution transmission electron microscopy and elemental analysis, showing that at short exposure times, Al2O3 accumulates at the top of the membrane, reducing pore size and creating a strong growth gradient, while at long exposure time, more homogeneous growth occurs. This detailed characterization creates the knowledge necessary for controlling the deposition gradient and achieving an efficient growth with minimum pore clogging. By tuning the Al2O3 exposure time and cycles, we demonstrate control over the Al2O3 depth gradient and membranes pore size, hydrophilicity, and permeability. The oil antifouling performance of membranes is investigated using in situ confocal imaging during flow. This characterization technique reveals that Al2O3 surface modification reduces oil droplet surface coverage.
更多查看译文
关键词
atomic layer deposition, membranes, ultrafiltration, oxide, gradient, transmission electron microscopy
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要