Effect of Initial Microstructure on the Properties of K439b Superalloy During Prolonged Aging at 800 °C Zesheng Liu,Chuanwei Li,Anping Dong,Jianfeng Gucrossref(2024)引用 0|浏览3暂无评分AI 理解论文溯源树样例生成溯源树,研究论文发展脉络Chat Paper正在生成论文摘要