Different laser damage testing protocols, including 1 -on -1, S -on -1, and Raster Scan, were conducted on 532 nm polarizers to evaluate the damage resistance and mechanisms. A comparison of the laser -induced damage thresholds (LIDTs) revealed different damage characteristics and major contributions to film failure for different polarizations. For P polarization, the LIDTs for the three test protocols were nearly the same because of the stabilization of two typical damage morphologies of flat-bottomed pits and mussel damage pits. For S polarization, the LIDTs for multiple pulses were lowest, where absorptive defect -induced damage was revealed. The damage characteristics of 532 nm polarizers and 1064 nm polarizers have been also compared. The mussel damage pits, which are similar to the typical damage morphologies of ultraviolet (UV) laser damage to fused silica, were observed for the first time in coatings of 532 nm polarizers. This suggests that, the polishing -induced subsurface damage of fused silica substrates may tend to be excited by a short -wavelength laser rather than the fundamental wavelength.
更多
查看译文
关键词
532 nm polarizer,1-on-1,S-on-1,Raster scan,LIDT,Damage morphologies
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要