Morphodynamics of dendrite growth in alumina based all solid-state sodium metal batteries

ENERGY & ENVIRONMENTAL SCIENCE(2023)

引用 0|浏览25
暂无评分
摘要
All solid-state batteries (ASSBs) with ceramic electrolytes and alkali metal anodes are a potential future energy storage technology for vehicle electrification and smart grids. However, uncontrollable dendrite growth toward ultimate short circuiting in solid electrolytes (SEs) has become a serious concern in the design of long-cycle, safe ASSBs, and the underlying mechanism has remained unclear. Here through multiscale imaging and morphodynamic tracking we show that Na dendrites grow in beta ''-Al2O3 SEs through an alternating sequence of Na deposition and crack propagation. Atomic-scale imaging evidenced that electrochemical cycling causes massive delamination cracking along the Na+ conduction planes, accompanied by the closure of neighboring conduction channels. In situ SEM observations revealed a dynamic interplay between Na deposition and crack propagation: Na deposition accumulates mechanical stress that induces cracking; cracking releases the local stress, which promotes further Na deposition. Thus, Na deposition and cracking alternatingly proceed until short circuits take place. A multiscale phase-field model is developed to recapitulate the morphodynamics of Na dendrite growth, predicting the tree-like fractal morphology of the growing dendrites. Our findings suggest that decoupling between Na deposition and cracking represents an important route to mitigate uncontrollable dendrite growth in ASSBs.
更多
查看译文
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要