Green energy storage devices play vital roles in reducing fossil fuel emissions and achieving carbon neutrality by 2050. Growing markets for portable electronics and electric vehicles create tremendous demand for advanced lithium-ion batteries (LIBs) with high power and energy density, and novel electrode material with high capacity and energy density is one of the keys to next-generation LIBs. Silicon-based materials, with high specific capacity, abundant natural resources, high-level safety and environmental friendliness, are quite promising alternative anode materials. However, significant volume expansion and redundant side reactions with electrolytes lead to active lithium loss and decreased coulombic efficiency (CE) of silicon-based material, which hinders the commercial application of silicon-based anode. Prelithiation, preembedding extra lithium ions in the electrodes, is a promising approach to replenish the lithium loss during cycling. Recent progress on prelithiation strategies for silicon-based anode, including electrochemical method, chemical method, direct contact method, and active material method, and their practical potentials are reviewed and prospected here. The development of advanced Si-based material and prelithiation technologies is expected to provide promising approaches for the large-scale application of silicon-based materials. & COPY; 2022 Institute of Process Engineering, Chinese Academy of Sciences. Publishing services by Elsevier B.V. on behalf of KeAi Communications Co., Ltd. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).
更多
查看译文
关键词
Si-based materials,Prelithiation,Coulombic efficiency,Lithium loss,Lithium-ion battery
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要