Effect of microstructure on the high cycle fatigue behaviour of DP 600 and SPFH 590 steels with and without a hole

Sudin Chatterjee, M. Chinara,A. D. Prasad, B. Jayabalan, V Mahashabde,S. Mukherjee

MATERIALS SCIENCE AND TECHNOLOGY(2021)

引用 1|浏览1
暂无评分
摘要
The performance of ferrite-martensite (DP 600) and ferrite-pearlite (SPFH 590) steels with a similar tensile strength of similar to 650 MPa under cyclic loading was investigated. This work presents the high cycle fatigue properties of DP 600 and SPFH 590 steel in the presence and absence of a hole. In presence of the hole, the fatigue strength for both the steels drops significantly, with drop being more for SPFH 590 steel. While the fatigue strength in absence of a hole is a strong function of yield strength of material, the behaviour in presence of the hole depends on the steel microstructure. The presence of martensite in case of DP 600 steel delayed the crack propagation by branching and crack tip blunting. Additionally, martensite also increases the local strain, low angle grain boundary and dislocation density ahead of the crack tip, resulting in an increased amount of plastic deformation and blunting of the crack tip.
更多
查看译文
关键词
High cycle fatigue, drilled hole, microstructure, advanced high-strength steels, fatigue crack
AI 理解论文
溯源树
样例
生成溯源树,研究论文发展脉络
Chat Paper
正在生成论文摘要